Gold elution circuit leaching: acid wash and carbon regeneration steps
A gold elution circuit removes precious metal from activated carbon after adsorption in a carbon-in-leach (CIL) or carbon-in-pulp (CIP) plant. The sequence must release gold efficiently, protect carbon activity, and produce a pregnant eluate suitable for electrowinning. Acid washing and thermal regeneration are essential supporting stages rather than optional maintenance tasks.
The circuit typically includes loaded-carbon screening, acid washing, water rinsing, alkaline elution, pregnant-solution handling, electrowinning, carbon drying, and kiln regeneration. The correct arrangement depends on ore mineralogy, cyanide chemistry, carbon quality, scale formation, and the selected stripping technology.
What the circuit must accomplish
During cyanidation, dissolved gold forms a stable complex that is adsorbed onto activated carbon. Once the carbon reaches its working loading, it is transferred from the adsorption tanks to the elution area. Screens remove slurry and fine solids before the carbon enters the acid-wash column.
The purpose of the overall circuit is to separate gold from carbon while keeping both streams valuable. Gold should report to a concentrated eluate for recovery at the electrowinning cells, while regenerated carbon should return to the adsorption circuit with sufficient pore volume and surface activity.
Poor circuit design can create several losses. Incomplete stripping leaves gold on carbon, excessive heat can damage the carbon structure, and inadequate washing can carry acid or dissolved contaminants into the elution stage. These problems reduce adsorption performance and complicate reagent control.
Acid washing loaded carbon
Acid washing removes inorganic deposits that block carbon pores or interfere with elution. Common contaminants include calcium carbonate, magnesium compounds, iron precipitates, copper minerals, and other scale-forming materials. Hydrochloric acid is widely used because it dissolves carbonate scale effectively, although the concentration and contact time must be established through testing.
Loaded carbon is usually screened and rinsed before acid is introduced. The wash may be performed in a dedicated column with upward or downward flow, depending on the plant design. The solution should move evenly through the carbon bed so that scale is removed throughout the column rather than only from preferential flow channels.
Acid wash solution must be isolated from cyanide-bearing streams. Contact between acid and cyanide can generate highly toxic hydrogen cyanide gas, so interlocks, drainage segregation, ventilation, gas monitoring, and validated operating procedures are fundamental. After the acid stage, the carbon is rinsed thoroughly with process water until the residual acidity is controlled.
Acid washing does not strip gold as its primary function. It prepares the carbon for efficient alkaline elution by opening blocked pores and removing mineral deposits. Frequent washing without evidence of scaling can increase chemical consumption and carbon attrition, while insufficient washing can cause progressively weaker gold recovery.
Elution and pregnant eluate recovery
After rinsing, the cleaned carbon enters the stripping stage. Two widely used approaches are the Zadra process and the Anglo American Research Laboratory (AARL) process. Both use heated alkaline solution, often containing sodium hydroxide, with cyanide conditions selected to promote desorption of the gold complex from carbon.
In a Zadra circuit, hot eluant circulates continuously through the carbon bed and then through the recovery system. AARL elution commonly uses a pre-soak with caustic and cyanide followed by hot-water elution and solution transfer. Pressure, temperature, flow rate, cyanide concentration, and cycle duration must be matched to the carbon loading and plant configuration.
The pregnant eluate passes to electrowinning cells, where gold is deposited onto cathodes or steel wool. The recovered sludge is then washed, filtered, dried, and smelted into doré. Solution balance is important because excessive dilution lowers gold concentration and increases the volume that must be heated and circulated.
| Circuit stage | Main purpose | Typical control focus | Common warning sign |
|---|---|---|---|
| Carbon screening | Remove slurry and fine solids | Screen aperture, spray water, carbon transfer rate | High solids carryover |
| Acid wash | Dissolve mineral scale and inorganic foulants | Acid strength, temperature, contact time, rinse quality | High pressure drop or slow elution |
| Alkaline elution | Desorb gold from activated carbon | Temperature, caustic level, cyanide, flow, cycle time | High residual gold on stripped carbon |
| Electrowinning | Recover gold from pregnant eluate | Current density, voltage, solution conductivity | Low cathode grade or unstable current |
| Carbon drying | Prepare carbon for thermal treatment | Moisture removal, airflow, residence time | Uneven kiln temperature |
| Thermal regeneration | Restore adsorption capacity | Kiln temperature, retention time, atmosphere | Low adsorption activity or excess attrition |
Thermal regeneration and carbon quality
Stripped carbon still contains organic fouling, residual process chemicals, and physically blocked pores. Thermal regeneration restores adsorption performance by heating the carbon in a controlled atmosphere, commonly with steam or limited oxygen. The carbon is usually dried first, then passed through a rotary kiln or vertical regeneration furnace.
Regeneration temperatures are often in the range of approximately 600–750°C, although the correct setpoint depends on carbon type, kiln design, residence time, and the nature of the foulants. Too little heat leaves organic matter in the pores. Excessive temperature or oxygen exposure can burn carbon, reduce particle strength, and increase losses through attrition.
After leaving the kiln, the carbon should be cooled without uncontrolled air contact while it remains hot. It is then screened to remove fines and returned to the adsorption circuit. Carbon samples should be evaluated for activity, hardness, particle-size distribution, ash content, and gold loading before and after regeneration.
Carbon management is closely linked to plant performance. Fresh carbon addition may be required to replace attrition losses, but a high replacement rate can indicate rough transfer systems, excessive hydraulic force, poor screening, or aggressive regeneration conditions.
Variables that reveal circuit performance
A reliable elution operation depends on measurements taken at each stage rather than a single final recovery figure. Operators should track loaded-carbon gold grade, stripped-carbon gold grade, acid consumption, eluate volume, eluate gold concentration, electrowinning recovery, carbon activity, and carbon loss.
Temperature is particularly important because desorption kinetics improve as the eluant becomes hotter, within the limits of the equipment and carbon stability. Flow distribution is equally significant. A short-circuiting path through the carbon bed can produce apparently normal flow while leaving much of the carbon insufficiently contacted.
The relationship between ore properties and adsorption behavior should be established before final equipment selection. Comparative CIL and CIP testing can help define carbon loading, transfer frequency, preg-robbing tendencies, and the likely stripping duty for a specific oxide gold ore.
| Performance indicator | What it helps diagnose | Useful response |
|---|---|---|
| High residual gold after elution | Inadequate temperature, contact, chemistry, or flow | Review cycle profile and sample carbon by bed depth |
| Rising acid consumption | Increased scale formation or contaminated water | Check ore chemistry, water quality, and wash frequency |
| Low eluate gold concentration | Excess dilution or weak loading | Review carbon transfer and solution balance |
| Falling carbon activity | Incomplete regeneration or organic fouling | Adjust kiln conditions and investigate foulant sources |
| High carbon fines | Attrition, poor screening, or excessive thermal stress | Inspect pumps, screens, valves, and kiln operation |
Recommendations for plant design and operation
Elution equipment should be selected as part of the complete gold recovery flowsheet. A supplier with capabilities spanning process testing, equipment supply, engineering, and commissioning can coordinate the acid-wash column, elution vessel, heat exchanger, electrowinning cells, kiln, pumps, instrumentation, and safety systems. Lozova presents integrated mineral processing equipment for projects requiring coordinated recovery plant packages.
- Confirm acid-wash chemistry and scale behavior with representative carbon and process-water samples.
- Define elution temperature, pressure, reagent strength, and cycle duration through laboratory or pilot testwork.
- Separate acid, cyanide, pregnant eluate, barren solution, and wash-water drainage systems.
- Install reliable temperature, flow, pressure, level, and conductivity instrumentation with alarm and interlock functions.
- Track carbon activity and attrition alongside gold recovery so deterioration is identified before production losses become severe.
Operators should also establish sampling points before and after acid washing, elution, regeneration, and adsorption. A practical sampling program makes it easier to distinguish a chemistry problem from a hydraulic problem or a carbon-quality problem. Commissioning should include water runs, reagent verification, instrument calibration, and controlled testing with loaded carbon.
A well-designed circuit turns carbon into a managed recovery medium rather than a consumable that is simply moved between tanks. For mine developers and plant operators, early testwork and integrated engineering reduce uncertainty in equipment sizing, reagent use, energy demand, and gold accounting.
Move from testwork to production
Gold elution circuit leaching works best when acid washing, alkaline stripping, electrowinning, and carbon regeneration are designed as one operating system. The right sequence protects carbon activity, concentrates gold into a recoverable solution, and supports stable plant performance across changing ore conditions.
Review your ore, carbon, water chemistry, and recovery objectives with a qualified process engineering team, then develop the testwork and equipment package needed for a safe, efficient elution circuit.